Academia.eduAcademia.edu

Figure 4. Hysteresis loops for the subsequent stretching ranges of a weft-knitted fabric plated with elastomeric yarn (variant 1).  Figure 2. a) View of the face of a weft-knitted fabric plated with elastomeric yarns, b) Schematic record of the stitch of a weft-knitted fabric plated with elastomeric yarns. Fabric properties: wale density  Pk =190/10 cm, course density Pr = 340/10 cm, surface density M = 260 g/m’.

Figure 4 Hysteresis loops for the subsequent stretching ranges of a weft-knitted fabric plated with elastomeric yarn (variant 1). Figure 2. a) View of the face of a weft-knitted fabric plated with elastomeric yarns, b) Schematic record of the stitch of a weft-knitted fabric plated with elastomeric yarns. Fabric properties: wale density Pk =190/10 cm, course density Pr = 340/10 cm, surface density M = 260 g/m’.